Combinations of natural rubber (NR), butadiene rubber (BR), and reclaim rubber (RR) were prepared with a view to producing low-cost re-treading materials. It was found that cure time and scorch time decreased with the increase in the reclaim content. Only a small reduction in the properties was observed in almost all systems upon the addition of 30 phr of reclaim rubber. Systems with good abrasion resistance and tensile strength were obtained. High tensile values of 22.8 and 20.1 MPa were able to obtain for the NR-rich system. Tear strength can be enhanced by the addition of reclaim rubber. Elongation at break was higher for all the systems even after adding 30 phr of RR. Modulus and compression set values were increased with RR loading. The thermal behavior and activation energy of NR/BR/RR blends were improved by the addition of RR. The phase morphology of the blends was studied using a scanning electron microscope.
자료의 정보 및 내용의 진실성에 대하여 해피캠퍼스는 보증하지 않으며, 해당 정보 및 게시물 저작권과 기타 법적 책임은 자료 등록자에게 있습니다. 자료 및 게시물 내용의 불법적 이용, 무단 전재∙배포는 금지되어 있습니다. 저작권침해, 명예훼손 등 분쟁 요소 발견 시 고객센터의 저작권침해 신고센터를 이용해 주시기 바랍니다.
해피캠퍼스는 구매자와 판매자 모두가 만족하는 서비스가 되도록 노력하고 있으며, 아래의 4가지 자료환불 조건을 꼭 확인해주시기 바랍니다.
파일오류
중복자료
저작권 없음
설명과 실제 내용 불일치
파일의 다운로드가 제대로 되지 않거나 파일형식에 맞는 프로그램으로 정상 작동하지 않는 경우