등통로각압축공정을 이용하여 제작된 Cu-15wt.%Ag 미세복합재료의 미세구조 및 기계적, 전기적 특성 (Mechanical and Electrical Properties of Cu-15wt.%Ag Microcomposites Processed by Equal Channel Angular Pressing)
한국학술지에서 제공하는 국내 최고 수준의 학술 데이터베이스를 통해 다양한 논문과 학술지 정보를 만나보세요.
Equal channel angular pressing (ECAP) with intermediate heat treatment was employed to optimize the strength of Cu-15 wt.%Ag. Changes in microstructure, electrical properties and mechanical properties were studied as a function of pressing methods and heat treatment. ECAPed Cu-15wt.%Ag exhibited ultrafine-grained microstructures with the shape and distribution of Ag-rich lamellae dependent on the processing routes. For route A in which the sample was pressed without rotation between each pass, the initial dendrites of Ag-rich phase were elongated along the shear direction and developed into elongated filaments. For route C in which the sample was rotated by 180 degree after each pass, the morphology of initial dendrites of Ag-rich phase was not much modified and the networked structure remained even after 8 passes of ECAP. For route Bc in which the sample was rotated by 90 degree after each pass, the initial dendrites became finer by fragmentation with no pronounced change of the shape and distribution of Ag-rich lamellae.
The strength of Cu-15wt.%Ag ECAPed using route Bc was found to be greater than those ECAPed using route A, suggesting that the substructural strengthening is more effective in strengthening than the interface strengthening.
영어초록
Equal channel angular pressing (ECAP) with intermediate heat treatment was employed to optimize the strength of Cu-15 wt.%Ag. Changes in microstructure, electrical properties and mechanical properties were studied as a function of pressing methods and heat treatment. ECAPed Cu-15wt.%Ag exhibited ultrafine-grained microstructures with the shape and distribution of Ag-rich lamellae dependent on the processing routes. For route A in which the sample was pressed without rotation between each pass, the initial dendrites of Ag-rich phase were elongated along the shear direction and developed into elongated filaments. For route C in which the sample was rotated by 180 degree after each pass, the morphology of initial dendrites of Ag-rich phase was not much modified and the networked structure remained even after 8 passes of ECAP. For route Bc in which the sample was rotated by 90 degree after each pass, the initial dendrites became finer by fragmentation with no pronounced change of the shape and distribution of Ag-rich lamellae.
The strength of Cu-15wt.%Ag ECAPed using route Bc was found to be greater than those ECAPed using route A, suggesting that the substructural strengthening is more effective in strengthening than the interface strengthening.
자료의 정보 및 내용의 진실성에 대하여 해피캠퍼스는 보증하지 않으며, 해당 정보 및 게시물 저작권과 기타 법적 책임은 자료 등록자에게 있습니다. 자료 및 게시물 내용의 불법적 이용, 무단 전재∙배포는 금지되어 있습니다. 저작권침해, 명예훼손 등 분쟁 요소 발견 시 고객센터의 저작권침해 신고센터를 이용해 주시기 바랍니다.
해피캠퍼스는 구매자와 판매자 모두가 만족하는 서비스가 되도록 노력하고 있으며, 아래의 4가지 자료환불 조건을 꼭 확인해주시기 바랍니다.
파일오류
중복자료
저작권 없음
설명과 실제 내용 불일치
파일의 다운로드가 제대로 되지 않거나 파일형식에 맞는 프로그램으로 정상 작동하지 않는 경우